Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 140 - 150 °C | 284 - 302 °F | |
Lubrizol Advanced Materials Pearlbond® 12C75 Thermoplastic Polyurethane Pearlbond® 12C75 is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low softe.. |
|||
Zone 3 | 140 - 150 °C | 284 - 302 °F | |
Lubrizol Advanced Materials Pearlthane® 12C75 Thermoplastic Polyurethane Elastomer Pearlthane® 12C75 is a standard polyester based TPU supplied in form of translucent, colorless pellets, specially designed for compounds in which TPU is used as an additive. Features include low .. |
|||
Zone 3 | 140 - 150 °C | 284 - 302 °F | |
Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane Pearlbond™ 125H is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low soft.. |
|||
Zone 3 | 130 - 150 °C | 266 - 302 °F | |
Solvay Specialty Polymers Cogegum® GFR/380 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Zone 3 | 130 - 150 °C | 266 - 302 °F | |
Fainplast Compounds HAX HFX 024-15C Halogen Free PVC This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linkable by heat and moisture by previous addition of a suitable catalyst masterbatch. It is recommended to s.. |
|||
Zone 3 | 130 - 150 °C | 266 - 302 °F | |
Fainplast Compounds HAX HFX 024-21L Halogen Free PVC This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linking by heat and moisture by previous addition of a suitable catalyst masterbatch. It is highly recommende.. |