Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 350 °C | 662 °F | Compression |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Zone 2 | 350 °C | 662 °F | Compression |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
Zone 2 | 350 °C | 662 °F | Compression |
BASF Ultrason® E 2010 MR HP PESU Description: Unreinforced, medium viscosity standard injection molding grade for improved demolding behavior with Mold Release. PES-Blend with improved processibility. (High Productivity) Abbreviate.. |
|||
Zone 2 | 350 °C | 662 °F | Compression |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |