Polymer Property : Zone 2 = 360 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 182 °C
360 °F
DuPont Nucrel® 535 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 535 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Zone 2 182 °C
360 °F
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for..
Zone 2 182 °C
360 °F
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Zone 2 182 °C
360 °F
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2806 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for..
Zone 2 182 °C
360 °F
DuPont Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Zone 2 182 °C
360 °F
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Zone 2 182 °C
360 °F
Extrusion
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane
Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection ..
Zone 2 182 °C
360 °F
Extrusion
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane
Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf..
Zone 2 182 °C
360 °F
Extrusion
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane
Features: Highly Elastic Compound and Good Recovery for a Rubber-Like CharacterUses: Flat Die/Film Extrusion and Blown Film and Injection Molding and Profile ExtrusionAvailable in Americas, Europe, ..
Zone 2 182 °C
360 °F
Extrusion
Lubrizol ESTANE® 58810 Ether Based Thermoplastic Polyurethane
Features: High melt flow and improved temperature resistanceUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by ..
Zone 2 182 °C
360 °F
Extrusion
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane
Features: Very high tensile strength, excellent low temperature flexibility, and superior abrasion and cut resistanceUses: Extrusion – Wire and cable, Hose and tube & General purposeAvailable in Am..
Zone 2 182 °C
360 °F
Extrusion
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab..
Zone 2 182 °C
360 °F
DuPont Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Zone 2 182 °C
360 °F
DuPont Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Zone 2 182 °C
360 °F
Extrusion
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane
Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai..
Zone 2 182 °C
360 °F
Extrusion
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: ..