Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 182 °C | 360 °F | |
DuPont Nucrel® 535 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 535 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 2 | 182 °C | 360 °F | |
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Zone 2 | 182 °C | 360 °F | |
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 2 | 182 °C | 360 °F | |
DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2806 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Zone 2 | 182 °C | 360 °F | |
DuPont Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 2 | 182 °C | 360 °F | |
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 2 | 182 °C | 360 °F | Extrusion |
Lubrizol ESTANE® 58219 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance, low temperature performance and clarity. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection .. |
|||
Zone 2 | 182 °C | 360 °F | Extrusion |
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf.. |
|||
Zone 2 | 182 °C | 360 °F | Extrusion |
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane Features: Highly Elastic Compound and Good Recovery for a Rubber-Like CharacterUses: Flat Die/Film Extrusion and Blown Film and Injection Molding and Profile ExtrusionAvailable in Americas, Europe, .. |
|||
Zone 2 | 182 °C | 360 °F | Extrusion |
Lubrizol ESTANE® 58810 Ether Based Thermoplastic Polyurethane Features: High melt flow and improved temperature resistanceUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by .. |
|||
Zone 2 | 182 °C | 360 °F | Extrusion |
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane Features: Very high tensile strength, excellent low temperature flexibility, and superior abrasion and cut resistanceUses: Extrusion – Wire and cable, Hose and tube & General purposeAvailable in Am.. |
|||
Zone 2 | 182 °C | 360 °F | Extrusion |
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab.. |
|||
Zone 2 | 182 °C | 360 °F | |
DuPont Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 2 | 182 °C | 360 °F | |
DuPont Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 2 | 182 °C | 360 °F | Extrusion |
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai.. |
|||
Zone 2 | 182 °C | 360 °F | Extrusion |
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: .. |