Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 100 - 120 °C | 212 - 248 °F | Compression |
Lubrizol Advanced Materials Pearlbond® Eco D900 Thermoplastic Polyurethane Pearlbond™ ECO D900 is a linear, aromatic polyurethane based on specialty polyol from renewable sources. It contains 67% of renewable material as certified according to ASTM-D6866. It is suppli.. |
|||
Zone 2 | 100 °C | 212 °F | |
Borealis LE0520 Polyethylene Compound, Crosslinkable, Semiconductive LE0520 is a Strippable Semi conductive Insulation Shielding for Power Cables. LE0520 is suitable for use in triple extrusion processes. Strip forces in the range of 3-6 kN/m (7-14 lbs/half inch) ha.. |