Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 340 - 360 °C | 644 - 680 °F | |
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Zone 1 | 340 - 360 °C | 644 - 680 °F | |
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Zone 1 | 340 °C | 644 °F | Feed zone |
BASF Ultrason® E 2010 MR SW 10111 PESU Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF |
|||
Zone 1 | 340 °C | 644 °F | Feed zone |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
Zone 1 | 340 °C | 644 °F | Feed zone |
BASF Ultrason® E 2010 MR HP PESU Description: Unreinforced, medium viscosity standard injection molding grade for improved demolding behavior with Mold Release. PES-Blend with improved processibility. (High Productivity) Abbreviate.. |
|||
Zone 1 | 340 °C | 644 °F | Feed zone |
BASF Ultrason® E 2010 SW Q31 10088 PESU Information provided by BASF |