Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66 Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H G3 15% Glass Reinforced PA66 Description: Nilamid A3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 66. This product combines good overall mechanical performance and impact strength with ease of processing.Key char.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66 Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H G4 General Purpose 20% Glass Reinforced PA66 Description: Nilamid A3 H G4 is a general purpose, 20% glass fiber reinforced NYLON 66. This product combine good overall mechanical performance and impact strength with ease of processing.Key chara.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It .. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66 Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66 Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66 Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66 Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66 Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H7 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H7 G6 is a 30% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | hopper |
Nilit Nilamid A3 H7 G7 35% Glass Reinforced PA66 Description: Nilamid A3 H7 G7 is a 35% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc.. |
|||
Zone 1 | 260 - 290 °C | 500 - 554 °F | hopper |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Zone 1 | 240 - 290 °C | 464 - 554 °F | |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Zone 1 | 240 - 290 °C | 464 - 554 °F | |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Zone 1 | 240 - 290 °C | 464 - 554 °F | |
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re.. |
|||
Zone 1 | 250 - 290 °C | 482 - 554 °F | |
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f.. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Staramide RB006S PA66, 30% Glass Bead Filled, Injection Molded Staramide RB006S is a 30% Glass Bead Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 30K S3)Information provided by Eurostar. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Starflam RF0059 PA66, Glass Fiber, Flame Retardant, Injection Molded Starflam RF0059 is a Flame Retardant, Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 270 - 290 °C | 518 - 554 °F | |
Eurostar Starflam RF0069 PA66, 30% Glass Fiber, Flame Retardant, Injection Molded Starflam RF0069 is a Flame Retardant, 30% Glass Reinforced Polyamide 66 Injection Molding Resin (also known as PA66 30V U2 Z79 or RF1006Z590)Information provided by Eurostar. |