Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 300 °C | 572 °F | Zone 1 |
Premix Thermoplastics PRE-ELEC® PC/ABS 1420 PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR.. |
|||
Die Temperature | 300 °C | 572 °F | Zone 4 |
Premix Thermoplastics PRE-ELEC® PC/ABS 1420 PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR.. |
|||
Die Temperature | 300 °C | 572 °F | Zone 5 |
Premix Thermoplastics PRE-ELEC® PC/ABS 1420 PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR.. |
|||
Die Temperature | 300 °C | 572 °F | Extrusion Coating |
DuPont™ Nucrel® 30705 Ethylene Acrylic Acid Nucrel® 30705 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethyle.. |
|||
Die Temperature | 300 - 320 °C | 572 - 608 °F | |
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU)
(Unverified Data**) Veradel 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |