Polymer Property : Die Temperature = 265 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 250 - 265 °C
482 - 509 °F
Celanese Celanex® 5200-2 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.15% glass reinforced, high gloss, general purpose, lubricatedInfor..
Die Temperature 250 - 265 °C
482 - 509 °F
Celanese Celanex® 5202 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Die Temperature 250 - 265 °C
482 - 509 °F
Celanese Celanex® 5300-2 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 5300-2 is a 30% fiberglass reinforced polyester with improved surface finish. Celanex 5300-2 contains an internal lubricant.30% glass reinforced, high gloss, general purpose, lubricatedInfor..
Die Temperature 240 - 265 °C
464 - 509 °F
Celanese Celanex® 6500 PBT, 30% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability.30% glass/mineral, low warpInformation provided by Celanese
Die Temperature 250 - 265 °C
482 - 509 °F
Celanese CELANEX 5200-2 PBT, 15% Glass Reinforced
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.Information provided by Celanese
Die Temperature 250 - 265 °C
482 - 509 °F
Celanese CELANEX 5300-2 PBT, 30% Glass Reinforced
Celanex 5300-2 is a 30% fiberglass reinforced polyester with improved surface finish. Celanex 5300-2 contains an internal lubricant.Information provided by Celanese
Die Temperature 250 - 265 °C
482 - 509 °F
Celanese Celanex® 5202HF PBT, 15% Glass Reinforced
Celanex 5202HF is a 15% glass-filled polyester featuring improved surface gloss and high flow for long flow channels. A typical application is oven handles.Information provided by Celanese Corporat..
Die Temperature 240 - 265 °C
464 - 509 °F
Celanese Celanex® 6407HR PBT, 30% Mineral / Glass Reinforced
Celanex 6407HR is a 30% glass/mineral reinforced hydrolysis resistant polyester particularly suited for large exterior automotive components where extended flow, flatness, and good surface appearanc..
Die Temperature 240 - 265 °C
464 - 509 °F
Celanese Celanex® 6500LM PBT, 30% Mineral / Glass Reinforced
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability, that is also enhanced for improved laser marking graphics.T..
Die Temperature 240 - 265 °C
464 - 509 °F
Celanese CELANEX 6407 PBT, 30% Mineral / Glass Reinforced
Celanex 6407 is a 30% glass/mineral reinforced resin perticularly suited for large exterior automotive components, where extended flow, flatness and good surface appearance is essential.Information ..
Die Temperature 240 - 265 °C
464 - 509 °F
Celanese CELANEX 6500 PBT, 30% Mineral / Glass Reinforced
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability.Information provided by Celanese
Die Temperature 250 - 265 °C
482 - 509 °F
Celanese Celanex® 5300-2UV PBT, 30% Glass Reinforced
Information provided by Celanese Corporation.
Die Temperature 240 - 265 °C
464 - 509 °F
Celanese Celanex® 6406 PBT, 40% Mineral / Glass Reinforced
Celanex 6406 is a 40% mineral/glass reinforced resin providing excellent toughness combined with warpage resistance, surface gloss and good mechanical properties. Celanex 6406 is particularly suited..
Die Temperature 250 - 265 °C
482 - 509 °F
Celanese CELANEX 5202 PBT, 15% Glass Reinforced
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Die Temperature 240 - 265 °C
464 - 509 °F
Celanese Celanex® 6407 PBT, 30% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6407 is a 30% glass/mineral reinforced resin perticularly suited for large exterior automotive components, where extended flow, flatness and good surface appearance is essential.30% glass/mi..
Die Temperature 240 - 265 °C
464 - 509 °F
Celanese Celanex® J600 PBT, 40% Mineral / Glass Reinforced  (Unverified Data**)
Celanex J-600 is a 40% glass/mineral reinforced resin providing excellent warpage resistance, surface gloss and good mechanical properties. Celanex J-600 is particularly suited to applications requi..
Die Temperature 240 - 265 °C
464 - 509 °F
Celanese CELANEX J600 PBT, 40% Mineral / Glass Reinforced
Celanex J-600 is a 40% glass/mineral reinforced resin providing excellent warpage resistance, surface gloss and good mechanical properties. Celanex J-600 is particularly suited to applications requi..