Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 240 °C | 464 °F | Zone 1 |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
Die Temperature | 240 °C | 464 °F | Zone 1 |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Die Temperature | 240 °C | 464 °F | Zone 1 |
Premix Thermoplastics PRE-ELEC® PE 1294 PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Die Temperature | 240 °C | 464 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Die Temperature | 240 °C | 464 °F | Cast Film |
Honeywell Aegis™ HCA73MP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA73MP is a lubricated and nucleated low viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 C.. |
|||
Die Temperature | 240 °C | 464 °F | Cast Film |
Honeywell Aegis™ HCA95YP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA95YP is a lubricated medium viscosity, nylon 6/6,6 film extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.. |
|||
Die Temperature | 240 °C | 464 °F | Tubular (Blown) Film |
Honeywell Aegis™ HCA115ZP Nylon 6/6,6 Extrusion Grade Copolymer
(discontinued **) Description: Aegis HCA115ZP is a high viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500. It possess.. |
|||
Die Temperature | 240 - 250 °C | 464 - 482 °F | |
Arkema Group OREVAC® 18319 Grafted Maleic Anhydride Polyethylene OREVAC 18319 is a maleic anhydride grafted polyethylene used in the manufacturing of multi-layer aluminium panels. OREVAC 18319 is mainly used in aluminium panels to have good adhesion performances .. |
|||
Die Temperature | 240 °C | 464 °F | |
Arkema Group OREVAC® 18370 Maleic Anhydride Modified Polyethylene OREVAC® 18370 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Die Temperature | 240 °C | 464 °F | |
Arkema Group OREVAC® 18365 Maleic Anhydride Modified Polyethylene OREVAC® 18365 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Die Temperature | 240 °C | 464 °F | |
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, DAM Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced .. |