Processing Properties Metric English Comments
Die Temperature 216 - 238 °C
421 - 460 °F
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE)
Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene..
Die Temperature 216 - 238 °C
421 - 460 °F
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE)
Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o..
Die Temperature 216 °C
420 °F
Extrusion
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Die Temperature 216 °C
420 °F
Extrusion
ExxonMobil Santoprene® 243-50 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Die Temperature 216 °C
420 °F
Extrusion
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Die Temperature 216 - 232 °C
420 - 450 °F
Extrusion
ExxonMobil Santoprene® 281-87MED Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad..
Die Temperature 216 °C
420 °F
Extrusion
ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Die Temperature 216 °C
420 °F
Extrusion
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
Die Temperature 216 - 221 °C
420 - 430 °F
LyondellBasell Petrothene® GA808093 Linear Low Density Polyethylene
ApplicationsPETROTHENE GA 808-093 is a broad molecular weight, linear low density polyethylene resin designed for use as a wire and cable insulation. An antioxidant package is added to ensure therm..
Die Temperature 216 °C
421 °F
6, Zone 1, Extrusion
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket..
Die Temperature 216 °C
421 °F
Zone 2, Extrusion
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket..
Die Temperature 216 °C
420 °F
Extrusion
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Die Temperature 216 °C
420 °F
Extrusion
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Die Temperature 216 °C
420 °F
Extrusion
ExxonMobil Santoprene® 123-40 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
Die Temperature 216 °C
420 °F
Extrusion
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Die Temperature 216 °C
420 °F
Extrusion
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Die Temperature 216 °C
420 °F
Extrusion
ExxonMobil Santoprene® 203-50 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Die Temperature 216 °C
420 °F
Extrusion
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer  (discontinued **)
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
Die Temperature 216 - 232 °C
421 - 450 °F
ExxonMobil Santoprene® 8291-85TL Thermoplastic Elastomer
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to create multilayer constructions offering bonding to textiles,..