Processing Properties Metric English Comments
Die Temperature 213 °C
415 °F
AdvanSource Biomaterials ChronoFlex® AL 55D Biodurable Medical Grade Polyurethane
ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by  AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade el..
Die Temperature 213 °C
415 °F
AdvanSource Biomaterials ChronoFlex® AL 65D Biodurable Medical Grade Polyurethane
ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas..