Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 177 - 216 °C | 351 - 421 °F | Extrusion |
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Die Temperature | 177 - 199 °C | 350 - 390 °F | |
Lubrizol Advanced Materials PEARLTHANE® 12K85LB Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K85 LB is a standard polyester-based TPU with a lubricating additive, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mech.. |
|||
Die Temperature | 177 °C | 350 °F | |
LyondellBasell Aquathene® AQ120000 Ethylene Vinylsilane Copolymer ApplicationsAQUATHENE AQ 120-000 is an ethylene vinylsilane copolymer designed for use in low voltage, power cable applications. This natural resin can be crosslinked, by exposure to moisture after.. |
|||
Die Temperature | 177 °C | 350 °F | |
LyondellBasell Aquathene® CM04482 Catalyst Masterbatch ApplicationsAQUATHENE CM 04482 is a catalyst masterbatch designed for use with AQUATHENE AQ 120-000 ethylene vinylsilane copolymer. When CM 04482 is added at 5 wt% to AQ 120-000, the resulting mate.. |
|||
Die Temperature | 177 °C | 350 °F | |
LyondellBasell Aquathene® CM92949B Black Masterbatch ApplicationsAQUATHENE CM 92949 is a black masterbatch designed for use with AQUATHENE AQ 120-00 ethylene vinylsilane copolymer for producing low voltage, power insulation. When CM 92949 is added at.. |
|||
Die Temperature | >= 177 °C | >= 350 °F | |
Borealis Visico™ LE4421/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation LE4421/LE4432 is a black, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a VISICO™ base material, LE4.. |
|||
Die Temperature | >= 177 °C | >= 350 °F | |
Borealis Visico™ LE4421/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4421/LE4437 is a natural, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a Visico base materi.. |
|||
Die Temperature | >= 177 °C | >= 350 °F | |
Borealis Visico™ LE4421/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4421/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination o.. |
|||
Die Temperature | >= 177 °C | >= 350 °F | |
Borealis Visico™ LE4423/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4423/LE4432 is a black, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a Visico base material.. |
|||
Die Temperature | >= 177 °C | >= 350 °F | |
Borealis Visico™ LE4423/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4423/LE4437 is a mature, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a Visico base materia.. |
|||
Die Temperature | >= 177 °C | >= 350 °F | |
Borealis Visico™ LE4423/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4423/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination o.. |
|||
Die Temperature | 177 - 188 °C | 351 - 370 °F | Zone 2, Extrusion |
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and.. |
|||
Die Temperature | >= 177 °C | >= 350 °F | |
Borealis Visico™ LE4421/LE4460/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4421/LE4460/LE4432 is a black, halogen-based flame retardant, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The.. |
|||
Die Temperature | 177 - 216 °C | 350 - 420 °F | Extrusion |
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Die Temperature | 177 °C | 350 °F | |
Axiall HHP-190 Rigid PVC, Extrusion Georgia Gulf HHP-190 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Heat Resistance & Thermal StabilityImpact Strength & ToughnessDimensi.. |
|||
Die Temperature | 177 °C | 350 °F | |
Axiall HHW-191 Rigid PVC, Extrusion Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic.. |
|||
Die Temperature | >= 177 °C | >= 350 °F | |
Borealis Visico™ LE4423/LE4460/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4423/LE4460/LE4432 is a black, halogen-based flame retardant, moisture-induced crosslinking polyethylene compound that is designed for use as low wire insulation and jacketing. The combina.. |
|||
Die Temperature | 177 - 216 °C | 350 - 420 °F | Extrusion |
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer
(discontinued **) A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance .. |