Polymer Property : Adapter Temperature = 225 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Adapter Temperature 210 - 225 °C
410 - 437 °F
Petroquimica Triunfo Trithene® TS 7001 LDPE - Heavy Duty Low Friction Film
The Trithene TS 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and low coefficient of fricti..
Adapter Temperature 210 - 225 °C
410 - 437 °F
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight
The Trithene TX 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and environmental stress crac..
Adapter Temperature 210 - 225 °C
410 - 437 °F
Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film
The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Sinc..