Polymer Property : Adapter Temperature = 195 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Adapter Temperature 180 - 195 °C
356 - 383 °F
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film
The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 78 E 4506 TPU-Polyester
Introduction: IROGRAN A 78 E 4506 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester
Introduction: IROGRAN A 85 E 4607 is a thermoplastic polyether- polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent mechan..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester
Introduction: IROGRAN A 85 H 4508 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are excellent mechanical properties and hig..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether
Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether
Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 85 P 4722 TPU-Polyester
Introduction: IROGRAN A 85 P 4722 is a halogen-free thermoplastic- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are good microbial resista..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry
Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 95 R 4813 is a thermoplastic polyester- polyurethane for injection moulding applications. Additional characteristics of the product are very short cycle times and high dimens..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 98 E 4066 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo..
Adapter Temperature 185 - 195 °C
365 - 383 °F
Extrusion
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester
Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester
Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 92 E 4694 is a thermoplastic special- polyester-polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and ..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h..
Adapter Temperature 175 - 195 °C
347 - 383 °F
Extrusion
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e..
Adapter Temperature 180 - 195 °C
356 - 383 °F
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade
The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,..