Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 25.0 °C | 77.0 °F | |
Honeywell Aegis™ OX High Barrier Nylon
(discontinued **) Description: Aegis OX is an oxygen-scavenging nylon. Oxygen barrier is comparable to a glass bottle with metal crown closure. In addition Aegis OX provides CO2 barrier and possesses glass-like cla.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 60 DB Thermoplastic Polyurethane Introduction: AVALON 60 DB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DB is part of the AVALON Perform Range and offers a premium soling materi.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 75 ABX Thermoplastic Polyurethane Introduction: AVALON 70 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 70 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 80 ABU Thermoplastic Polyurethane Introduction: AVALON 80 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABU is part of the AVALON Perform Range and offers a premi.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling .. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 98 AB Thermoplastic Polyurethane Introduction: AVALON 98 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 98 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 98 AE Thermoplastic Polyurethane Introduction: AVALON 98 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 98 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Feed Temperature | 25.0 - 45.0 °C | 77.0 - 113 °F | Injection |
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Feed Temperature | 25.0 - 45.0 °C | 77.0 - 113 °F | Injection |
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 95 E 4861 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A95 4861 is a high performance polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN A95E 4861 is part of the HUNTSMAN technical extrusion pro.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 65 ABX Thermoplastic Polyurethane Introduction: AVALON 65 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 65 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 70 AE Thermoplastic Polyurethane Introduction: AVALON 70 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 70 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 90 AK Thermoplastic Polyurethane Introduction: AVALON 90 AK is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same har.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 90 AKU Thermoplastic Polyurethane Introduction: AVALON 90 AKU is a part of the AVALON Crystal Range and offers a specially designed, flexible material wit a higher degree of transparency compared with conventional TPU at the same ha.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 91 P 4945 TPU-Polyester Introduction: IROGRAN A 91 P 4945 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 91 P 4945 is part of the HUNTSMAN technical ext.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN .. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi.. |