Feed Temperature |
60.0 - 70.0 °C |
140 - 158 °F |
Injection molding |
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance
Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value.. |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB50 NL PBT, unfilled, natural, high viscosity
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, heat stabilized, black
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, improved impact, heat stabilized, black
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 CR30 BK111 PBT, 30% carbon fiber reinforced, black
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 GB30 NL PBT, 30% glass bead reinforced, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 GR15 BK EF PBT, 15% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 GR15 BK002 WX21 PBT, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 GR15 NL100 KA01 PBT/PET, 15% glass fiber reinforced, heat stabilized, natural, gas injection grade
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 GR15 NL100 PBT, 15% glass fiber reinforced, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 GR20 NL100 XA20 PBT, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 GR30 NL SV20 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 GR30 NL XA70 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 GR50 BK009 MX01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, improved impact, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 NL RT PBT, unfilled, PTFE modified, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 NL TD22 PBT/PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecopet® PT70 GR15 NL100 PR PET, 15% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecopet® PT70 GR30 NL100 HT PET, 30% glass fiber reinforced, high heat stabilized, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 GR30 NL100 PBT, 20% glass fiber reinforced, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 GR40 NL100 PBT, 40% glass fiber reinforced, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 GR45 NL100 HS01 PBT/PET, 45% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecodur® PB70 NL SV20 PBT, unfilled, flame retardant - halogen (RoHS compliant), natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecopet® PT70 GR45 NL100 PR PET, 45% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecopet® PT74 GR20 BK002 DA PET, 20% glass fiber reinforced, high heat stabilized, black
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
Throat |
Eurotec® Tecopet® PT74 GR45 BK002 PR PET, 45% glass fiber reinforced, high heat stabilized, black
Information provided by Eurotec® |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
|
3M Dyneon™ PFE 300Z Clear Perfluoroelastomer System
Features and Benefits:Proprietary polymer and catalyst system enables the manufacture of optically clear finished partsProportionate polymer and catalyst package simplifies the mixing processLow ext.. |
Feed Temperature |
50.0 - 70.0 °C |
122 - 158 °F |
|
3M Dyneon™ 301Z Translucent Perfluoroelastomer System
Features and Benefits:Excellent plasma resistance with low particle count Low extractables, low outgassing, and low particle generation for ultra high purity applicationsPhosphorous-free and silica.. |