Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Feed Temperature = 419 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Feed Temperature 200 - 215 °C
392 - 419 °F
Lubrizol Estane® S160D Thermoplastic Polyurethane
Type: Estane® S160D is a Shore 63D, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
Feed Temperature 200 - 215 °C
392 - 419 °F
Lubrizol Estane® S360D Thermoplastic Polyurethane
Type: Estane® S360D is a Shore 63D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi..
Feed Temperature 200 - 215 °C
392 - 419 °F
Lubrizol Estane® S364D Thermoplastic Polyurethane
Type: Estane® S364D is a Shore 65D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi..