Polymer Property : Feed Temperature = 392 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Feed Temperature 185 - 200 °C
365 - 392 °F
Lubrizol Estane® S195A Thermoplastic Polyurethane
Type: Estane® S195A is a Shore 95A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
Feed Temperature 185 - 200 °C
365 - 392 °F
Lubrizol Estane® L194A Thermoplastic Polyurethane
Type: Estane® L194A is a Shore 95A, polyester grade thermoplastic polyurethane (TPU).Uses: Injection Molding.Availability: AsiaInformation Provided by The Lubrizol Corporation