Polymer Property : Feed Temperature = 265 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Feed Temperature 260 - 265 °C
500 - 509 °F
Lavergne VYPET VNT 335 PET 35% Glass - Mineral Reinforced
Vypet VNT 335 is a 35% glass/mineral reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityT..
Feed Temperature 255 - 265 °C
491 - 509 °F
Solvay TECHNYL® A 218G V33 Black 41N PA66, 33% glass fiber, DRY
Description: TECHNYL® A 218G V33 Black 41N is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This pr..
Feed Temperature 255 - 265 °C
491 - 509 °F
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY
Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod..
Feed Temperature 260 - 265 °C
500 - 509 °F
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, Conditioned
Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition..
Feed Temperature 260 - 265 °C
500 - 509 °F
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15..
Feed Temperature 260 - 265 °C
500 - 509 °F
Solvay TECHNYL® 2417IG PA66, 20% glass fiber, DRY
Description: Polyamide 66, 20% glass fiber reinforced, Impact modified for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2417IG4 is used in all sectors of industries,..
Feed Temperature 260 - 265 °C
500 - 509 °F
Solvay TECHNYL® 2912GMH7-P PA66, 63% glass fiber, DRY
Description: Polyamide 66, reinforced with 63% of glass fiber for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2912GMH7-P is used in all sectors of industry, offerin..