Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 175 - 185 °C | 347 - 365 °F | |
NatureWorks® Ingeo™ AW 300D Injection Grade Biopolymer Specifically designed for use in injection molded food serviceware applications. This opaque, off-white molding grade creates parts that are rigid and heat resistant for tableware used with hot food.. |
|||
Feed Temperature | 170 - 185 °C | 338 - 365 °F | |
Petroquimica Triunfo Trithene® TS 7001 LDPE - Heavy Duty Low Friction Film The Trithene TS 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and low coefficient of fricti.. |
|||
Feed Temperature | 170 - 185 °C | 338 - 365 °F | |
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight The Trithene TX 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and environmental stress crac.. |
|||
Feed Temperature | 170 - 185 °C | 338 - 365 °F | |
Petroquimica Triunfo Trithene® TU 3001 LDPE - Agricultural Film The Trithene TU 3001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical properties, good processability and bu.. |
|||
Feed Temperature | 170 - 185 °C | 338 - 365 °F | |
Petroquimica Triunfo Trithene® TU 8091 LDPE - Agricultural Film Trithene TU 8091 is a low-density polyethylene (LDPE) with high molecular weight, with excellent mechanical properties and good processability. These qualities ensure the production of very wide fil.. |
|||
Feed Temperature | 175 - 185 °C | 347 - 365 °F | |
Lavergne VYSTYRENE PS 3904 High Impact Polystyrene Vystyrene PS 3904 is a black impact modified polystyrene compound with balanced impact/stiffness properties designed for injection molding applicationsFeatures: -High resilience -Excellent process.. |
|||
Feed Temperature | 175 - 185 °C | 347 - 365 °F | |
Lavergne VYSTYRENE PS 3901 High Impact Polystyrene Vystyrene PS 3901 is a black impact modified polystyrene compound with balanced impact/stiffness properties designed for injection molding applicationsFeatures: -High resilience -Excellent process.. |
|||
Feed Temperature | 170 - 185 °C | 338 - 365 °F | |
Lubrizol Estane® T470A Thermoplastic Polyurethane Type: Estane® T470A is a Shore 77A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Feed Temperature | 170 - 185 °C | 338 - 365 °F | |
Petroquimica Triunfo Trithene® TX 4003 LDPE and LLDPE Blend - High Resistance Film The Trithene® TX 4003 resin is a blend of low-density polyethylene (LDPE) of high molecular weight with linear low-density polyethylene (LLDPE) designed for the production of industrial films. Sinc.. |
|||
Feed Temperature | 170 - 185 °C | 338 - 365 °F | |
Lubrizol Estane® S175A Thermoplastic Polyurethane Type: Estane® S175A is a Shore 77A, polyester type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mid.. |