Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 76.7 - 93.3 °C @Time 14400 - 86400 sec |
170 - 200 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman 710H Utility Black ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 87.8 - 93.3 °C @Time 7200 - 86400 sec |
190 - 200 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman 710H Utility Black ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 76.7 - 93.3 °C @Time 14400 - 86400 sec |
170 - 200 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman 720H Black ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 87.8 - 93.3 °C @Time 7200 - 86400 sec |
190 - 200 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman 720H Black ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 76.7 - 93.3 °C @Time 14400 - 86400 sec |
170 - 200 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman 730H White ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 87.8 - 93.3 °C @Time 7200 - 86400 sec |
190 - 200 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman 730H White ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 76.7 - 93.3 °C @Time 14400 - 86400 sec |
170 - 200 °F @Time 4.00 - 24.0 hour |
Tray Dryer |
Shuman 780H Grey ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Drying Temperature | 87.8 - 93.3 °C @Time 7200 - 86400 sec |
190 - 200 °F @Time 2.00 - 24.0 hour |
Dehumidifying Dryer |
Shuman 780H Grey ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |