Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 99999 min

@Temperature 25.0 °C
99999 min

@Temperature 77.0 °F
Indefinite working life at 25°C (100 g)
Armstrong A-701 Epoxy Adhesive
A one-component, light gray, thixotropic, non-sag epoxy adhesive. A-701 uses an inert oxide filler that provides excellent electrical insulation properties. Features high temperature, 400°F, bond..
Pot Life 99999 min

@Temperature 25.0 °C
99999 min

@Temperature 77.0 °F
Indefinite working life at 25°C (100 g)
Armstrong A-702 Epoxy Adhesive
Information provided by Ellsworth Adhesives.
Pot Life 99999 min

@Temperature 25.0 °C
99999 min

@Temperature 77.0 °F
Indefinite working life at 25°C (100 g)
Armstrong A-706 Epoxy Adhesive
A one-component, gray, aluminum-filled, thixotropic, non-sag epoxy adhesive. A-706 has an in-service temperature range to 400°F, but requires 350°F minimum cure temperature. Features excellent m..