Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 840 min | 840 min | Less if accelerated |
Abatron TDS, AboThane 861019/8606-5 Acrylic/Polyurethane Enamel
(discontinued **) Acrylic/polyurethane highest-grade glossy colored enamel for metal, plastics, concrete, wood, floors and structures indoor and outdoor. Rule 66 exempt. 2-component system for superior performance .. |
|||
Pot Life | 840 min @Temperature 25.0 °C |
840 min @Temperature 77.0 °F |
|
Abatron AboCast/AboCure 50-24/8501-4 High Temperature Resistant Epoxy Clear amber, low viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to.. |