Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 60 - 75 min | 60 - 75 min | 100 grams |
Master Bond EP21LVMed Two Component, Low Viscosity USP Class VI Epoxy Master Bond EP21LVMed is a two component, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is formulated to cure readily at room tempera.. |
|||
Pot Life | 60 - 75 min | 60 - 75 min | 200 gram mass |
Master Bond EP21TDCN Two Component Nickel Conductive Epoxy Adhesive Product Description: Master Bond Polymer System EP21TDCN is a two component, nickel filled, electrically conductive, adhesive for high performance bonding, formulated to cure at room temperature or .. |
|||
Pot Life | 60 - 75 min | 60 - 75 min | 200 gram mass |
Master Bond EP21TDCNFL Two Component Nickel Conductive Epoxy Adhesive Master Bond Polymer System EP21TDCNFL is a two component, nickel filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
Pot Life | 60 - 75 min | 60 - 75 min | 100 gram mass |
Master Bond EP21TDCSFL Flexible Two Component Silver Conductive Epoxy Master Bond Polymer System EP21TDCSFL is a two component, silver filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
Pot Life | 45 - 75 min | 45 - 75 min | 100 gram batch |
Master Bond EP42HT-2Med Epoxy Meets USP Class VI Requirements Description: Master Bond Polymer System EP42HT-2Med is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along wit.. |
|||
Pot Life | 60 - 75 min | 60 - 75 min | 100 gm mass |
Master Bond EP79FL Two Component Silver Nickel Conductive Epoxy Adhesive Master Bond Polymer System EP79FL is a two component, silver-coated nickel, electrically conductive system for high performance bonding and sealing. Its most salient features are its high flexibilit.. |
|||
Pot Life | 60 - 75 min | 60 - 75 min | 100 gram mass |
Master Bond EP21CLV Two Component Epoxy System Product Description: Master Bond EP21CLV is a two component, lower viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting. It features easy handling a.. |
|||
Pot Life | 60 - 75 min | 60 - 75 min | 100 gram batch |
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo.. |
|||
Pot Life | 45 - 75 min | 45 - 75 min | 100 gram mass |
Master Bond EP30M4 Chemically Resistant Two Component Epoxy System Master Bond Polymer System EP30M4 is a two component epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weight. EP30M4 resi.. |
|||
Pot Life | 45 - 75 min | 45 - 75 min | 100 gram batch |
Master Bond EP42HT-2 Epoxy Adhesive Resists Sterilization Description: Master Bond Polymer System EP42HT-2 is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material featuring high temperature resistance along with o.. |
|||
Pot Life | 45 - 75 min | 45 - 75 min | 100 gram batch |
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications Master Bond Polymer System EP42HT-2FG is a room temperature setting, two component epoxy adhesive, sealant and coating specially formulated for food applications. It has been independently tested an.. |
|||
Pot Life | 60 - 75 min | 60 - 75 min | |
Abatron AboCoat 8006-3/8606-3 Clear Versatile Epoxy Clear epoxy protective and dielectric coatings. For spraying, brushing or rolling on metal, concrete, masonry, wood, fiberglass and most surfaces. Good adhesion, flexibility, hardness, water and c.. |
|||
Pot Life | 45 - 75 min | 45 - 75 min | 100 gram mass |
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to.. |
|||
Pot Life | 45 - 75 min | 45 - 75 min | 100 gram batch |
Master Bond EP42HT-2LO Low Outgassing, Heat Resistant Two Component Epoxy Master Bond Polymer System EP42HT-2LO is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along with outstanding .. |