Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | >= 720 min | >= 720 min | 100 gram batch |
Master Bond EP37-3FLSP Optically Clear Epoxy Has Low Exotherm Description: Master Bond EP37-3FLSP is a very flexible, low viscosity, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. It fe.. |
|||
Pot Life | >= 720 min | >= 720 min | 200 gram batch |
Master Bond EP45HTAO Heat Resistant Epoxy for Structural Bonding Description: Master Bond Polymer Compound EP45HTAO is a two component thermally conductive epoxy compound for high performance structural bonding, and casting. It is suitable for applications where .. |
|||
Pot Life | >= 720 min | >= 720 min | 1 quart mass |
Master Bond EP45HTAO Heat Resistant Epoxy for Structural Bonding Description: Master Bond Polymer Compound EP45HTAO is a two component thermally conductive epoxy compound for high performance structural bonding, and casting. It is suitable for applications where .. |
|||
Pot Life | 720 - 1440 min | 720 - 1440 min | 100 gram batch |
Master Bond EP45HTND-2 Chemically Resistant, Non-Drip Epoxy Description: Master Bond EP45HTND-2 is a two component epoxy system for high performance bonding, sealing and coating. It is used for applications requiring solid temperature resistance and capable .. |
|||
Pot Life | >= 720 min | >= 720 min | 200 gram batch |
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy Description: Master Bond Polymer Compound EP45HTQ is a two component quartz filled, epoxy compound for high performance structural bonding and casting. It is suitable for applications where long ter.. |
|||
Pot Life | >= 720 min | >= 720 min | 1 quart mass |
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy Description: Master Bond Polymer Compound EP45HTQ is a two component quartz filled, epoxy compound for high performance structural bonding and casting. It is suitable for applications where long ter.. |
|||
Pot Life | 720 - 1440 min | 720 - 1440 min | 100 gram batch |
Master Bond EP46HT Epoxy Adhesive for Structural Bonding Description: Master Bond System EP46HT is a newly formulated two component high performance heat resistant epoxy resin system with excellent mechanical strength and chemically resistant properties f.. |
|||
Pot Life | >= 720 min | >= 720 min | 100 gm mass |
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi.. |
|||
Pot Life | >= 720 min | >= 720 min | 200 gram mass |
Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding Description: Master Bond Polymer Adhesive SUPREME 45HTND is a two component epoxy adhesive featuring a balance of shear and peel strengths for high performance structural bonding suitable for applic.. |
|||
Pot Life | >= 720 min | >= 720 min | 1 quart mass |
Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding Description: Master Bond Polymer Adhesive SUPREME 45HTND is a two component epoxy adhesive featuring a balance of shear and peel strengths for high performance structural bonding suitable for applic.. |
|||
Pot Life | 720 min | 720 min | |
Tra-Con Tra-Duct 2956 Low Ion Snap Cure Silver Epoxy Adhesive TRA-DUCT 2956 is recommended for the bonding and sealing of electronic components where a combination of electrical and mechanical properties are required. This two-part, smooth, paste system of sil.. |
|||
Pot Life | 720 min | 720 min | |
Abatron Primkote G A/B Waterborne Epoxy Primer/Sealer for Green Concrete Primkote G is a waterborne epoxy system for priming and sealing floors. It contains a gray resin compound (Part A) and a clear hardener (Part B). It conditions concrete and other substrates for epox.. |
|||
Pot Life | >= 720 min | >= 720 min | 1 quart mass |
Master Bond Supreme 46HT-2ND2 Two Component, Non-Drip, Toughened, Epoxy Adhesive Master Bond Polymer Supreme 46HT-2ND2 is a two component, non-drip, epoxy adhesive featuring an attractive balance of superior shear and peel strengths for high performance structural bonding suitab.. |
|||
Pot Life | >= 720 min | >= 720 min | 200 gram mass |
Master Bond Supreme 46HT-2ND2 Two Component, Non-Drip, Toughened, Epoxy Adhesive Master Bond Polymer Supreme 46HT-2ND2 is a two component, non-drip, epoxy adhesive featuring an attractive balance of superior shear and peel strengths for high performance structural bonding suitab.. |