Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 5.00 - 6.00 min | 5.00 - 6.00 min | |
Northstar Polymers MPP-M09D "Slow Cure" Semi-Rigid Foam Formulation This foam polyurethane formulation is designed yield structural foam by either hand-mixing or machine casting method. The pot-life of this material is set longer than ordinary rigid foam formulatio.. |