Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 360 min @Temperature 23.0 °C |
360 min @Temperature 73.4 °F |
2X Starting Viscosity |
Parker Chomerics THERM-A-FORM T644 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Pot Life | >= 360 min | >= 360 min | |
Abatron 2232 A/B Filled Potting Compound
(discontinued **) Lower viscosity filled potting, encapsulating, and casting system. Black and most colors. 4/1 variable ratio.Information provided by Abatron. |
|||
Pot Life | >= 360 min | >= 360 min | |
Abatron 4823A/50-17B Filled Potting Compound
(discontinued **) Gray or colors. 73% filled heat sink potting and encapsulating system. 100/6.6 ratio.Information provided by Abatron. |
|||
Pot Life | >= 360 min | >= 360 min | |
Abatron 7703-2A/5017B Filled Potting Compound
(discontinued **) Tan and colors dielectric heat sink paste with 65% alumina filler. 100/8 ratio.Information provided by Abatron. |
|||
Pot Life | 360 min @Temperature 25.0 °C |
360 min @Temperature 77.0 °F |
|
Momentive Performance Materials TSE3033 Clear General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
Pot Life | 360 - 480 min | 360 - 480 min | 200 gram batch |
Master Bond Super Gel 9AOND Dimensionally Stable Urethane Modified Epoxy Master Bond Super Gel 9AOND is a two component, urethane modified epoxy system that cures at room temperature and has a paste-like consistency. It offers softness and retains dimensional stability. .. |
|||
Pot Life | 360 min | 360 min | 25 grams |
Tra-Con Tra-Bond 526M04 Color Keyed High Temperature Epoxy Adhesive TRA-BOND 526M04 is a low viscosity, high-temperature, two-part epoxy formulation with a long working life. TRA-BOND 526M04 exhibits excellent wicking, and develops strong, tough mechanically stable .. |
|||
Pot Life | 360 min | 360 min | |
Epoxy Technology EPO-TEK® 330 Low Viscosity, Optical Epoxy Product Description: EPO-TEK® 330 is a two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications.Advan.. |
|||
Pot Life | 360 min | 360 min | |
Epoxy Technology EPO-TEK® 360 Low Viscosity Optical Epoxy Adhesive Product Description: EPO-TEK® 360 is a two component, high-temperature grade epoxy for semiconductor, electronics, fiber optics and medical applications.Advantages & Application Notes: Built in col.. |
|||
Pot Life | 360 min | 360 min | |
Epoxy Technology EPO-TEK® E2116 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E2116 is a two component, silver-filled and stencil printable electrically conductive adhesive for bonding SMDs onto PCB and substrates. Can be used as a “lead-free”.. |
|||
Pot Life | >= 360 min | >= 360 min | |
Epoxyset Epoxibond EB-119M Unfilled Epoxy Adhesive A two-component,unfilled, low viscosity, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by.. |
|||
Pot Life | 360 - 480 min @Temperature 25.0 °C |
360 - 480 min @Temperature 77.0 °F |
100 g |
Abatron AboCast 10-5/AboCure 50-17 Epoxy AboCast 10-5 is a filled, high-viscosity epoxy resin. It is blended with AboCure 50-17 to make a structural adhesive and casting compound for the optic and electric industry. AboCure 50-17 is a high.. |
|||
Pot Life | 360 min @Temperature 360 °C |
360 min @Temperature 680 °F |
500 g |
Abatron AboCast 8103-16 One Part Epoxy One component system. Less viscous than 8103-11. Information provided by Abatron, Inc.Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 360 min. at 100°C (212°C). Peak e.. |