Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 17 - 24 min | 17 - 24 min | |
ITW Plexus Plexusâ„¢ MA422 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, medium open time.Information provided by Illinois Tool Works. |
|||
Pot Life | 17 - 24 min | 17 - 24 min | |
ITW Plexus Plexus™ MA922 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, medium open time.Information provided by Illinois Tool Works. |