Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 15.0 - 20.0 min | 15.0 - 20.0 min | |
Northstar Polymers MCP-V40A Polyurethane Gel MCP-V40A is a polyurethane gel formulation specifically designed for padding and cushioning applications, where low rebound property of the material is critical. This viscoelastic polymer is a two.. |
|||
Pot Life | 17.0 - 20.0 min | 17.0 - 20.0 min | |
Northstar Polymers MPA-A30B Mold-Making Resin MPA-A30B is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Pot Life | 15.0 - 20.0 min @Temperature 23.0 °C |
15.0 - 20.0 min @Temperature 73.4 °F |
|
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Pot Life | 15.0 - 20.0 min @Temperature 23.0 °C |
15.0 - 20.0 min @Temperature 73.4 °F |
|
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Pot Life | 15.0 - 20.0 min @Temperature 23.0 °C |
15.0 - 20.0 min @Temperature 73.4 °F |
|
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Pot Life | 15.0 - 20.0 min @Temperature 23.0 °C |
15.0 - 20.0 min @Temperature 73.4 °F |
|
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Pot Life | 15.0 - 20.0 min @Temperature 25.0 °C |
15.0 - 20.0 min @Temperature 77.0 °F |
1 lbm |
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Pot Life | 15.0 - 20.0 min @Temperature 25.0 °C |
15.0 - 20.0 min @Temperature 77.0 °F |
1 lbm |
Cytec EN-2534 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |