Polymer Property : Pot Life = 2.0 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 1.0 - 2.0 min
1.0 - 2.0 min
Time before parts must be mated
Lord Adhesives 202 Semi-Flexible, Fast Cure, Medium Viscosity Acrylic Adhesive
Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f..
Pot Life 1.0 - 2.0 min
1.0 - 2.0 min
ITW Plexus Plexusâ„¢ MA420FS Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, very fast curing.Information provided by Illinois Tool Works.