Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 135 min @Temperature 25.0 °C |
135 min @Temperature 77.0 °F |
|
Momentive Performance Materials RTV560 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |