Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Pot Life = 12 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 12 - 15 min
12 - 15 min
ITW Plexus Plexusâ„¢ MA3940 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with craze sensitive plastics.Information provided by Illinois Tool Works.
Pot Life 12 min
12 min
Taiwan PU Corporation PTMG CPU-42L Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Pot Life >= 12 min
>= 12 min
200 gram mass
Master Bond Supreme 46HT-2 Toughened, High Shear and Peel Strength Adhesive
Description: Master Bond Supreme 46HT-2 is a two component epoxy adhesive featuring an attractive balance of good shear and peel strengths for high performance structural bonding and coating suitabl..
Pot Life 12 - 14 min
12 - 14 min
Abatron AboWeld/AboCure 7812-2 Thixotropic Epoxy
AboWeld/AboCure 7812-2 is an underwater and cold-weather structural and dielectric adhesive paste. It is a 2-component thixotropic epoxy compound for dry, wet, and cold applications. It has many spe..
Pot Life 12 min

@Temperature 24.0 °C
12 min

@Temperature 75.2 °F
1 lb. mass
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting
BC8010-2 Metal-Kast/Slo, the result of extensive research and development is an aluminum filled, metal-like, medium setting urethane reproduction plastic. A slower version of the BC8010 Metal-Kast w..
Pot Life 12 - 14 min

@Temperature 24.0 °C
12 - 14 min

@Temperature 75.2 °F
mass dependent
BCC Products BC 8782 Urethane Casting
BC 8782 produces a high impact rigid 82 Shore D material that is commonly used to make clear or tinted castings of all kinds. When used at room temperature castings 1/8" thick or larger can be readi..
Pot Life 12 - 15 min

@Temperature 24.0 °C
12 - 15 min

@Temperature 75.2 °F
BCC Products BC 8880 Polyurethane Elastomer Surface Coat
BC8880 is a two-part urethane gel coat which exhibits excellent handling characteristics and very low moisture sensitivity. Its characteristics include a high modulus and a high hardness. It is a br..
Copyright © lookpolymers.com All Rights Reserved