Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 6.0 - 10 min | 6.0 - 10 min | anti-slump |
ACC QSil 430 QSI Quantum Silicones Silicone Potting Material
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: 100% solid, quick curing, flame retardant, great adhesion to a variety of substrates. |
|||
Pot Life | 6.0 - 10 min | 6.0 - 10 min | Time before parts must be mated |
Lord Adhesives 406 Flexible, High Impact and Peel Resistance, Medium Working Time Acrylic Adhesive Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e.. |
|||
Pot Life | 5.0 - 10 min | 5.0 - 10 min | Time before parts must be mated |
Lord Adhesives 710 Two-component, Equal mix, Non-Flammable Urethane Adhesive Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe.. |
|||
Pot Life | 6.0 - 10 min | 6.0 - 10 min | Time before parts must be mated |
Lord Adhesives 7500C Two-Component, 100% Solids Urethane Adhesive Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe.. |
|||
Pot Life | 5.0 - 10 min | 5.0 - 10 min | Time before parts must be mated |
Lord Adhesives 7520 Two-Component, Non-Sag Urethane Adhesive Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe.. |
|||
Pot Life | 5.0 - 10 min | 5.0 - 10 min | Time before parts must be mated |
Lord Adhesives 7540 Two-Component, 100% Solids, Equal Mix Urethane Adhesive Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe.. |
|||
Pot Life | 5.0 - 10 min | 5.0 - 10 min | 100 gram batch |
Master Bond EP51FL Toughened and Flexible Adhesive Compound Master Bond EP51FL is a two component epoxy system for high performance bonding sealing and coating. It combines superior toughness with user friendly handling properties, along with unusually fast .. |
|||
Pot Life | 5.0 - 10 min @Temperature 24.0 °C |
5.0 - 10 min @Temperature 75.2 °F |
1lb mass |
BCC Products BC 4553 Polyester Styling Paste BC4553 is designed for instant buildup and repair of plastic surfaces and models. Recommended for use on SMC and FRP parts, vacuum form molds and a variety of surfaces. When cured BC4553 produces a .. |
|||
Pot Life | 5.0 - 10 min @Temperature 24.0 °C |
5.0 - 10 min @Temperature 75.2 °F |
1 lb mass |
BCC Products BC 4578 Polyester Model Board Filler BC 4578 is a quick setting easy to use filler paste which is designed specifically for repair to Model Board MB 2001. Its lightweight characteristic and tack free cure makes for ease of finishing wi.. |
|||
Pot Life | 6.0 - 10 min @Temperature 24.0 °C |
6.0 - 10 min @Temperature 75.2 °F |
gel time |
BCC Products BC 4558 Polyester Filler Paste BC4558 is a unique quickset paste designed for aircraft use in making fast repairs to damaged metal surfaces. Also recommended for use in edge filling honeycomb core and foam core composite panels. .. |
|||
Pot Life | 8.0 - 10 min @Temperature 24.0 °C |
8.0 - 10 min @Temperature 75.2 °F |
1 lb. mass |
BCC Products BC 8165 Urethane Casting BC 8165 is a low viscosity, rapid setting, rigid urethane compound. This system will cure quickly to a hard, tough, impact resistant casting. BC 8165 is non-sensitive to moisture after cure and wil.. |