Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 0.33 min | 0.33 min | Open Time |
Valley Adhesives EM-220 Low Temperature Application Glue Stick Valley Adhesives EM-220 Low Temperature Application Glue StickBonds many plastics, polyolefins and light weight heat sensitive materials. |
|||
Pot Life | 0.33 min | 0.33 min | Open Time |
Valley Adhesives EM-700 High Temperature Application Glue Stick Valley Adhesives EM-700 High Temperature Application Glue StickRecommended for porous substrates; Bonds corrugated boxes, foam and carpeting. |