Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BA202E Polypropylene Block Copolymer for Non-Pressure Pipes BA202E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA202E is recommended for non-pressure pipes & fittings, thin-walled.. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BA204E Polypropylene Block Copolymer for Non-Pressure Pipes BA204E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA204E is recommended for non-pressure pipes & fittings, thin-walle.. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BB108E Polypropylene compound for Steel Pipe Coating BB108E is a high molecular weight, low melt flow rate polypropylene block copolymer. Applications: BB108E is recommended for steel pipe coating.Information provided by Borealis AG |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis Beta-PPR™ RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems Beta-PPR RA7050 is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof of t.. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis Beta-PPR™ RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems Beta-PPR RA7050-GN is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof o.. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis Borcoat™ BA213E Polypropylene for Steel Pipe Coating Borcoat™ BA213E is a polypropylene compound used as a component in thermal insulation coating systems. Applications: Borcoat™ BA213E is recommended as a polymer to make foam for thermal insulatio.. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis Borcoat™ BB108E-1199 White Polypropylene Block Copolymer for Steel Pipe Coating Borcoat BB108E-1199, a ready made white compound, is a highly molecular weight, low melt flow polypropylene block copolymer. As a top-coat in three component polypropylene systems, Borcoat BB108E-1.. |
|||
Head Temperature | 210 - 230 °C | 410 - 446 °F | |
Borealis BorECO™ BA2000 Polypropylene Block Copolymer for Non-Pressure Pipes BorECO™ BA2000 is a high molecular weight, low melt flow rate polypropylene block copolymer with a good balance of mechanical properties. This grade offers superior stiffness while keeping good im.. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BorECO™ BA212E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BA212E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high stiffness and impact strength.BorECO BA212E is recommended for solid wall and structured wal.. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BA222E is a high molecular weight, low melt flow rate polypropylene block copolymer with superior stiffness and excellent impact properties. BorECO BA222E fulfills the requirements according.. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BorECO™ BA415E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO™ BA415E is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength. This material has been designed for improved processability and.. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BorECO™ BEC5015 Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BEC5015 is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength.BorECO BEC5015 is recommended for solid wall and structured wall n.. |
|||
Head Temperature | >= 210 °C | >= 410 °F | |
Borealis Borstar® HE6067 Black Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables Borstar HE6067 is a black, bimodal, co-polymer high density polyethylene (HDPE) compound produced according to the bimodal Borstar process. It is characterized by its balanced properties important .. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E Polypropylene Random Copolymer RA130E is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is natural colored. Applications RA130E is recommended for the production of PP-R pipes and .. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-1498 Polypropylene Random Copolymer RA130E-1498 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is white colored. Applications: RA130E-1498 is recommended for the production of PP-R p.. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-6015 Polypropylene Random Copolymer RA130E-6015 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-6017 Polypropylene Random Copolymer RA130E-6017 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Head Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-6034 Polypropylene Random Copolymer RA130E-6034 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Head Temperature | 210 - 240 °C | 410 - 464 °F | Pipe Extrusion |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Head Temperature | 210 - 240 °C | 410 - 464 °F | Pipe Extrusion |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Head Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |