Processing Properties | Metric | English | Comments |
---|---|---|---|
Hot-Working Temperature | 190 - 200 °C | 374 - 392 °F | Average value: 195 °C Grade Count:5 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |