Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Cooling Temperature | 274 °C | 525 °F | |
Solvay Specialty Polymers Halar® 558 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® 558 fluoropolymer is a resin grade for foam extrusion applications, including primary insulations, coaxial cable cores, cross-webs, fire alarm cable, jackets, and foam tubing. Like other g.. |