Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Opening | 0.0635 - 0.150 cm | 0.0250 - 0.0591 in | Average value: 0.0812 cm Grade Count:9 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Die Opening | 0.100 - 0.150 cm | 0.0394 - 0.0591 in | Blow Film Extrusion |
Braskem TN2005 EVA General Film Copolymer TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e.. |
|||
Die Opening | 0.100 - 0.150 cm | 0.0394 - 0.0591 in | Blow Film Extrusion |
Braskem TN2006 EVA General Film Copolymer TN2006 is an Ethylene-Vinyl Acetate (EVA) copolymer with good mechanical properties, high flexibility and toughness even with low temperature, and excellent optical and heat sealability properties. .. |
|||
Die Opening | 0.100 - 0.150 cm | 0.0394 - 0.0591 in | Blow Film Extrusion |
Braskem TU3001 LDPE Blown Film Extrusion Polyethylene TU3001 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties, and good processability. These qualities ensure the production of films with uniform thicknes.. |
|||
Die Opening | 0.100 - 0.150 cm | 0.0394 - 0.0591 in | Blow Film Extrusion |
Braskem TU3002 LDPE Blown Film Extrusion Polyethylene TU3002 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties (dart drop and Elmendorf tear strength), and good processability. These qualities ensure the p.. |
|||
Die Opening | 0.100 - 0.150 cm | 0.0394 - 0.0591 in | Blow Film Extrusion |
Braskem TX7001 LDPE Blown Film Extrusion Polyethylene TX7001 is a low-density polyethylene (LDPE) with high molecular weight designed to satisfy those applications that require high mechanical strength and environmental stress cracking resistance (ESCR.. |