Polymer Property : Die Opening = 0.0591 in Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Opening 0.0635 - 0.150 cm
0.0250 - 0.0591 in
Average value: 0.0812 cm Grade Count:9
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Die Opening 0.100 - 0.150 cm
0.0394 - 0.0591 in
Blow Film Extrusion
Braskem TN2005 EVA General Film Copolymer
TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e..
Die Opening 0.100 - 0.150 cm
0.0394 - 0.0591 in
Blow Film Extrusion
Braskem TN2006 EVA General Film Copolymer
TN2006 is an Ethylene-Vinyl Acetate (EVA) copolymer with good mechanical properties, high flexibility and toughness even with low temperature, and excellent optical and heat sealability properties. ..
Die Opening 0.100 - 0.150 cm
0.0394 - 0.0591 in
Blow Film Extrusion
Braskem TU3001 LDPE Blown Film Extrusion Polyethylene
TU3001 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties, and good processability. These qualities ensure the production of films with uniform thicknes..
Die Opening 0.100 - 0.150 cm
0.0394 - 0.0591 in
Blow Film Extrusion
Braskem TU3002 LDPE Blown Film Extrusion Polyethylene
TU3002 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties (dart drop and Elmendorf tear strength), and good processability. These qualities ensure the p..
Die Opening 0.100 - 0.150 cm
0.0394 - 0.0591 in
Blow Film Extrusion
Braskem TX7001 LDPE Blown Film Extrusion Polyethylene
TX7001 is a low-density polyethylene (LDPE) with high molecular weight designed to satisfy those applications that require high mechanical strength and environmental stress cracking resistance (ESCR..