Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3020GX9 23% Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: 23% glass fiber reinforced gradeInformation provided by UBE. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3020IX1 Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, impact modifiedInformation provided by UBE. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3020X8 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030JLX2 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability Information provided by UBE. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 Description: UBESTA has a strong resistance to chemicalsInformation provided by UBE. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethylene Glycol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Acetic Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Fuel C/E10 for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Fuel C/E10 for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hexane for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hexane for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Xylene for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Methanol for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Die Opening | 0.0400 cm | 0.0157 in | For T-Die Cast Film Extrusion |
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |