Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 82.7 - 172 MPa | 12000 - 25000 psi | |
PTS Trimid® N6-G15HL 15% GFR Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 82.7 - 172 MPa | 12000 - 25000 psi | |
PTS Trimid® N6-G33L 33% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 82.7 - 172 MPa | 12000 - 25000 psi | |
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 82.7 - 124 MPa | 12000 - 18000 psi | Average value: 103 MPa Grade Count:6 |
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu.. |