Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 75.01 - 120.0 MPa | 10880 - 17400 psi | |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |