Processing Properties Metric English Comments
Injection Pressure 4.83 - 150 MPa
700 - 21800 psi
Average value: 73.3 MPa Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Injection Pressure 4.83 - 150 MPa
700 - 21800 psi
Average value: 76.2 MPa Grade Count:12
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe..
Injection Pressure 4.83 - 103 MPa
700 - 15000 psi
Average value: 53.6 MPa Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 1501
Description: Injection Molding GradeInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 1501E
Description: Extrusion GradeInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 1502
Description: Injection Molding Grade, High GlossInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3002MC
Description: Plating GradeInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3300
Description: General Purpose Utility BlackInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 6.21 MPa
700 - 900 psi
Diamond Polymers ABS 3500ELG
Description: Injection Molding Grade, Medium Impact, Low GlossInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3501
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3501 GF-30
Description: Reinforced Grade, 30%Glass FilledInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3501 Natural 1000 P
Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3501E
Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3501E Natural 1000 S
Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3502E
Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 6.21 MPa
700 - 900 psi
Diamond Polymers ABS 4000HH-ELG
Description: Heat Resistant Grade, Low Gloss, Medium High HeatInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 4001H3F
Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 4001HH
Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 7600B
Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 6.21 MPa
700 - 900 psi
Diamond Polymers ABS 7600B (ELG)
Description: Blow Molding Grade, Extra High Impact, Low GlossInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 7602B
Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 9501
Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS TM 40
Description: Heat Resistant Grade, Ultra High HeatInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS TX-541
Description: Super High Heat ABSInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS VP-11 SHF
Description: High Flow, Flame Retardant ABSInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers SE 3 HH
Description: High Heat ABSInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers TR 5000
Description: Transparent ABSInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers TR 5000 AS/P
Description: Transparent ABS, Antistatic GradeInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 7.58 MPa
700 - 1100 psi
Diamond Polymers ABS 3501 GF-20
Description: Reinforced Grade, 20%Glass FilledInformation provided by Diamond Polymers, Inc.
Injection Pressure 4.83 - 150 MPa
700 - 21800 psi
Average value: 61.7 MPa Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Copyright © lookpolymers.com All Rights Reserved