Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 4.83 - 150 MPa | 700 - 21800 psi | Average value: 73.3 MPa Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Injection Pressure | 4.83 - 150 MPa | 700 - 21800 psi | Average value: 76.2 MPa Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 1000 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 1501E Description: Extrusion GradeInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 1502 Description: Injection Molding Grade, High GlossInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3002MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3003 MC Description: High Heat Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3500 Natural 1050 Description: Natural, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 6.21 MPa | 700 - 900 psi | |
Diamond Polymers ABS 3500ELG Description: Injection Molding Grade, Medium Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3501 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3501 GF-30 Description: Reinforced Grade, 30%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3501 Natural 1000 P Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3501E Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 3502 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 4000HH Description: Heat Resistant Grade, Medium High HeatInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 4001H3F Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 4001HH Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 4003HH Description: Heat Resistant Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 7500E Description: Extrusion Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 7602B Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 9500B Description: Blow Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 9501 Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 9502 Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 9502E Description: Extrusion Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS TM 40 Description: Heat Resistant Grade, Ultra High HeatInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 6.21 MPa | 700 - 900 psi | |
Diamond Polymers ABS VP-11 ELG Description: Extrusion Grade, Low Gloss, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS VP-12 Description: Flame Retardant with UVInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers SE 3 HH Description: High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers TR 5000 AS/P Description: Transparent ABS, Antistatic GradeInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.83 - 7.58 MPa | 700 - 1100 psi | |
Diamond Polymers ABS 7501 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |