Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 4.14 - 7.58 MPa | 600 - 1100 psi | |
Diamond Polymers ABS 2510 Description: Injection Molding Grade, Medium Impact, Super High FlowInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.14 - 7.58 MPa | 600 - 1100 psi | |
Diamond Polymers ABS 2512 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.14 - 7.58 MPa | 600 - 1100 psi | |
Diamond Polymers ABS 3501 SHF Description: Super High FlowInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.14 - 6.21 MPa | 600 - 900 psi | Secondary |
Clariant 6008 L Nylon 6, High Impact, Injection Molding Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.14 - 7.58 MPa | 600 - 1100 psi | |
Diamond Polymers ABS 3501 HF Description: High FlowInformation provided by Diamond Polymers, Inc. |
|||
Injection Pressure | 4.14 - 7.58 MPa | 600 - 1100 psi | |
Diamond Polymers ABS 2510 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |