Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 20.7 - 48.3 MPa | 3000 - 7000 psi | Injection |
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane Features: Good Flexibility at Low Temperatures and Improved Weathering Performance.Uses: Flat Die/Cast Film Extrusion and Hose/Profile Extrusion, Injection Molding.Available in Americas, Europe, Mid.. |