Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 138 - 193 MPa | 20000 - 28000 psi | Average value: 165 MPa Grade Count:4 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |