Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 58.84 - 137.3 MPa | 8534 - 19910 psi | |
LG Chemical IF850 PMMA, General Purpose Grade for Injection Molding High flowability gradeParticularly recommended for complicated profiles or large and thin wall partsFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface har.. |
|||
Injection Pressure | 58.84 - 137.3 MPa | 8534 - 19910 psi | |
LG Chemical IF870S PMMA, General Purpose Grade for Injection Molding Highest flowability of all gradesFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface hardness and coloring propertySuperior electrical resistance and mecha.. |
|||
Injection Pressure | 78.45 - 137.3 MPa | 11380 - 19910 psi | |
Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Injection Pressure | 78.45 - 137.3 MPa | 11380 - 19910 psi | |
Kolon DIAMAT® EH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Injection Pressure | 78.45 - 137.3 MPa | 11380 - 19910 psi | |
Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Injection Pressure | 78.45 - 137.3 MPa | 11380 - 19910 psi | |
Kolon DIAMAT® GP Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Injection Pressure | 78.45 - 137.3 MPa | 11380 - 19910 psi | |
Kolon DIAMAT® IG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Injection Pressure | 78.45 - 137.3 MPa | 11380 - 19910 psi | |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Injection Pressure | 78.45 - 137.3 MPa | 11380 - 19910 psi | |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |