Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® SR-0310 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 58.80 - 108 MPa | 8528 - 15600 psi | |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 58.80 - 108 MPa | 8528 - 15600 psi | |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Injection Pressure | 68.6 - 108 MPa | 9950 - 15600 psi | |
Samsung Cheil Industries Starex® SR-0310 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |